Sign In | Join Free | My frbiz.com |
|
Categories | FeCrAl Alloy |
---|---|
Brand Name: | DLX |
Model Number: | 0Cr25Al5 |
Place of Origin: | China Jiangsu |
MOQ: | 5 |
Payment Terms: | L/C, T/T, Western Union, MoneyGram |
Supply Ability: | 500 tons per month |
Delivery Time: | 7-20 days |
Packaging Details: | Spool package with Carton box, Coil package with polybag for 0Cr25Al5 |
Material: | Ferrous Chromium Aluminum |
Resistivity: | 1.42+/-0.05 |
Tensile Strength: | 630-780MPA |
Elongtation: | ≥12% |
Application: | Heating, Resistivity |
Condition: | Hard / Soft |
Sureface: | Bright, Oxided, Acide |
Maximum Temperature: | 1250℃ |
Melting Point: | 1500℃ |
Name: | 0Cr25Al5 |
Certification: | CE,ROHS |
Company Info. |
Changzhou DLX Alloy Co., Ltd. |
Verified Supplier |
View Contact Details |
Product List |
2.5 mm FeCrAl Kan-A1 wire heat electrical element wire resistance heating wire 0Cr25AL5
Fe-Cr-Al alloy has the characteristic of high resistivity,low
temperature resistance coefficient,high operating temperature,good
anti-oxidation and anti-corrosion under high temperature.
It is widely used in industrial furnace, household appliances,
industry furnace, metallurgy, machinery, aircraft, automotive,
military and other industries producing heating elements and
resistance elements.
nichrome heating alloy includes pure nickel, NiCr alloy, Fe-Cr-Al
alloy and copper nickel alloy.
FeCrAl resistance wire grade: 0Cr25Al5, 1Cr13Al4, 0Cr23Al5,
0Cr27Al7Mo2, 0Cr21Al6Nb, 0Cr21Al4, 0Cr21Al6.
In the form of wire, ribbon and strip, one kind of material
Fe-Cr-Al alloy.
Wire: 0.018mm-10mm
Rod: 8mm-50mm
Ribbon: 0.05*0.2mm-2.0*6.0mm
Strip: 0.5*5.0mm-5.0*250mm
Alloy Nomenclature Performance | 1Cr13Al4 | 0Cr25Al5 | 0Cr21Al6 | 0Cr23Al5 | 0Cr21Al4 | 0Cr21Al6Nb | 0Cr27Al7Mo2 | |
Main Chemical composition | Cr | 12.0-15.0 | 23.0-26.0 | 19.0-22.0 | 20.5-23.5 | 18.0-21.0 | 21.0-23.0 | 26.5-27.8 |
Al | 4.0-6.0 | 4.5-6.5 | 5.0-7.0 | 4.2-5.3 | 3.0-4.2 | 5.0-7.0 | 6.0-7.0 | |
Re | opportune | opportune | opportune | opportune | opportune | opportune | opportune | |
Fe | Rest | Rest | Rest | Rest | Rest | Rest | Rest | |
Nb0.5 | Mo1.8-2.2 | |||||||
Max. continuous service temp. of element(°C) | 950 | 1250 | 1250 | 1250 | 1100 | 1350 | 1400 | |
Resistivity at 20ºC(μΩ·m) | 1.25 | 1.42 | 1.42 | 1.35 | 1.23 | 1.45 | 1.53 | |
Density(g/cm3) | 7.4 | 7.1 | 7.16 | 7.25 | 7.35 | 7.1 | 7.1 | |
Thermal conductivity(KJ/m·h·ºC) | 52.7 | 46.1 | 63.2 | 60.2 | 46.9 | 46.1 | ||
Coefficient of lines expansion(α×10-6/ºC) | 15.4 | 16 | 14.7 | 15 | 13.5 | 16 | 16 | |
Melting point approx.( ºC) | 1450 | 1500 | 1500 | 1500 | 1500 | 1510 | 1520 | |
Tensile strength(N/mm2) | 580-680 | 630-780 | 630-780 | 630-780 | 600-700 | 650-800 | 680-830 | |
Elongation at rupture(%) | >16 | >12 | >12 | >12 | >12 | >12 | >10 | |
Variation of area(%) | 65-75 | 60-75 | 65-75 | 65-75 | 65-75 | 65-75 | 65-75 | |
Repeat Bending frequency(F/R) | >5 | >5 | >5 | >5 | >5 | >5 | >5 | |
Hardness(H.B.) | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | |
Continuous Servicetime(Hours/ ºC) | -- | ≥80/1300 | ≥80/1300 | ≥80/1300 | ≥80/1250 | ≥50/1350 | ≥50/1350 | |
Micrographic structure | Ferrite | Ferrite | Ferrite | Ferrite | Ferrite | Ferrite | Ferrite | |
Magnetic properties | Magnetic | Magnetic | Magnetic | Magnetic | Magnetic | Magnetic | Magnetic |
![]() | ||
![]() | ||
![]() | ||
![]() | ||
![]() |
![]() |