Sign In | Join Free | My frbiz.com |
|
Categories | Tungsten Carbide Ball |
---|---|
Brand Name: | JN |
Model Number: | 4.76MM 9.525MM 3.56MM |
Certification: | ISO SGS |
Place of Origin: | China |
MOQ: | 500kg |
Price: | Negotiable |
Payment Terms: | L/C, D/A, D/P, T/T, Western Union, MoneyGram,Paypal |
Supply Ability: | 10tons per week |
Delivery Time: | 7-15 days |
Packaging Details: | Ploy bag+25kg carton box+1000kg wooden box |
Product Nam: | YG8 Tungsten Carbide Ball |
Size Range: | 0.3mm-90mm |
Type: | Power Tool Parts |
Material: | YG8 , YG8X , YG10 |
Feature: | higher hardness and wear resistance |
Application: | high-tech machinery industry |
G25 Tungsten Carbide Machinery Bearing Balls For Radio 4.76MM
9.525MM 3.56MM
Applications |
---|
Special and hydraulic precision valves, special bearings, couplers,
flow meters, sprayers, recirculating balls, ball spindles, tooling
machines, sliding rails, ballpoint pens, pin and tips for
indicators, precision measurement instruments, medical instruments.
They are used in naval, mining, petrol and coining industry. |
Type | %WC | %Co | - | - | - | - | - | - | - | - | - |
---|---|---|---|---|---|---|---|---|---|---|---|
WC30 | 91.00-93.00 | 7.00-9.00 | - | - | - | - | - | - | - | - | - |
Type | ISO | USA | CHN | - | - | - | - |
---|---|---|---|---|---|---|---|
WC30 | K30 | C2 | YG8 | - | - | - | - |
Property | Symbol | U.o.M. | Type | Notes | Values |
---|---|---|---|---|---|
Density | δ | [g/cm3] | Physical | Room temp. | 14.70 |
Young's modulus | E | [GPa] | Mechanical | - | 630 |
Specific heat | c | [J/kg-K] | Thermal | Room temp. | 227 |
Coefficient of linear thermal expansion | α | [10^-6/ºC] | Thermal | (ΔT=0-100°C) | 6.0 |
Thermal conductivity | λ | [W/(m·K)] | Thermal | Room temp. | 82.0 |
Electric resistivity | ρ | [Ω*m*10^-9] | Electric | - | 175 |
Relative magnetic permeability | µ | - | Magnetic | Slighlty ferrom. | max 12 |
Property | Type | U.o.M. | Values | U.o.M. | Values |
---|---|---|---|---|---|
Grain size | Physical | [µm] | 1.2 - 1.6 | - | - |
Hardness | Mechanical | [HRA] | 89.5 - 91.0 | [HV] | 1480 - 1700 |
Ultimate compressive strength | Mechanical | [MPa] | 5400 - 5700 | [psix10^3] | 784 - 826 |
Service temperature | Thermal | [ºC] | -196 / 500 | [ºF] | -320.8 / 932 |
Corrosion Resistance |
---|
As a general rule Tungsten Carbides with Cobalt binder show good
corrosion resistance into basic solution while they are not
resisting into acid solutions. |
![]() |