Sign In | Join Free | My frbiz.com |
|
Categories | Balustrade Glass |
---|---|
Brand Name: | Crystal Base |
Model Number: | TSG |
Certification: | CE/CSI/BS/ASTM |
Place of Origin: | China |
MOQ: | 100sqm |
Price: | negotiation |
Payment Terms: | T/T ,L/C,DP or western Union |
Supply Ability: | 3,000 Sqm per Day |
Delivery Time: | 15 days after order confirmed |
Packaging Details: | Packed in Strong Plywood Crates or Cases with PE,paper or Saftpad interlayer |
Product Name: | Safety Glass |
Application: | Window,Buliding;Glass balustrade;Table;Show shelves;Door, |
Size Of Panel: | Various |
Colours: | Clear,colorless,transparent;ultra clear |
Standard: | CE/CSI/BS/ASTM |
Type: | Flat or Curved Sheet Glass |
Thickness: | 3mm;4mm;5mm;6mm;8mm;10mm;12mm |
Transmittance: | more than 88% |
Transparent SGP Balustrade Glass Fence Panels , Heat Toughened Safety Glass
Specification:
me | glass laminated |
Size | Min. Size:250mm*250mm Max. size:2440mm*3660mm |
Thickness | Glass:3mm-12mm |
Application | Architectural door, window,ceiling, floor and curtain wall glass.exhibitions hall,Building glass. |
Production Range | Low-E glass ,tempered glass, insulated glass, laminated glass, reflective glass etc. |
Description
tempered glass is a heat toughened safety glass. It has undergone a special heat treatment to increase its strength and resistance to impact. In fact, large tempered glass is approximately five times more resistant than normal glass. As an example a piece of 8mm toughened glass will be able to withstand a steel ball weighing 500gr dropped from a height of 2 meters.
Tempered glass production process
1. Cutting : cutting the annealing glass to the actual needs of shape.
2. Glass edging: Edging machine to mill the four edges to prevent frund when steeling,while
maintaining the beautiful appearance.
3. Drilling hole:If need to drilling hole using drilling machine.
4. Washing dry:cleaning the glass with washing maching.
5. Tempered glass:Tempered glass is produced by heating annealed glass in a furnace to 700°,
then the glass is rapidly cooled with jets of cold air to 40°,through the procedures, the original
glass is formed of tempered glass.
![]() |